Under what conditions can spray welding be used?

author:admintime:2019-09-22 22:20click:
            Spray welding is to reheat the preheated self-soluble alloy powder coating to 1000-1300 C, melt the particles, float the slag onto the surface of the coating, and disperse the boride and silicide in the coating, so as to achieve good bonding between the particles and the surface of the substrate.
            Spray welding process is suitable for the following situations:
            1. Surface loads of various kinds of carbon and low alloy steels are large, especially those subjected to impact loads. For workpieces with bonding strength of 350-450N/mm2, spray welding hardness HRC150 < 65, coating thickness from 0.3 to several millimetres, and surface roughness of spray welding layer after grinding can reach Ra0.4-0.1 micrometres.
            2. When used in corrosive media, the coating is required to be compact and porous.
            3. Hardening, carburizing, nitriding and hard chromium plating are used in the original design of workpiece surface, which requires high hardness.
            4. Workpiece working environment is bad, such as strong abrasive wear, erosion wear, cavitation and so on.
            5. Oxygen-acetylene flame alloy powder spray welding process is suitable for surface strengthening or repairing of various carbon steel and low alloy steel parts, but some characteristics of parts material should be noticed. When the linear expansion coefficient of matrix material differs greatly from that of alloy spray welding layer, it should be used cautiously when the linear expansion coefficient of matrix material is less than 12 *10-6/~C and more than 12 *10-6/~C, so as to avoid manufacturing. Cracks can also be difficult to spray welding if the content of elements with high affinity to oxygen in matrix metals is more than 3%, the total content of elements such as tungsten and molybdenum is more than 0.5%, or the sulfur content in steel is more than 0.5%. This is because these materials are easy to form dense and stable oxide film by interaction with oxygen to prevent melting. The wetting effect of the alloy on the matrix will cause the liquid alloy to roll like a "sweat bead" during remelting. Therefore, the adaptability of the spray welding process to the sprayed matrix material should be paid attention to.
            6. Metal materials that can be sprayed without special treatment:
            7. Metal materials that need to be preheated at 250-375 C after spray welding need to be slowly cooled.
            8. Metal materials requiring isothermal annealing after spray welding

Telephone

0769-85415700

function

Price

quality

service

Wechat sweep

Mobile phone sweep

图片区小说区另类春色| 久在线中文字幕亚洲日韩| 久久久精品中文字幕乱码18 | 国产成人卡2卡3卡4乱码| 国产永久av福利在线观看| 精品亚洲一区二区三区在线观看 | 白嫩少妇bbw撒尿视频| 人妻少妇久久中文字幕456| 乱人伦人妻中文字幕无码久久网| 日本妇人成熟免费| 亚洲成av人片在一线观看 | 99国内精品久久久久久久| 亚洲欧美中文字幕在线一区| 日韩人妻中文无码一区二区七区 | 久久精品青草社区| 欧美成人免费视频一区二区 | 国产成a人亚洲精v品无码性色 | 免费看成人毛片无码视频| 不卡av电影在线| 国产免费牲交视频| 好日子在线观看视频大全免费动漫| 99九九99九九视频精品| 国内精品视这里只有精品| 亚洲乱码高清午夜理论电影| 中文字幕制服丝袜人妻动态图| 一本色道久久综合亚州精品蜜桃| 99久久亚洲精品无码毛片| 欧美另类在线制服丝袜国产| 五月开心播播网| 久久理论片午夜琪琪电影网| 亚洲精品一区二区三区精品| 国产精品白丝av嫩草影院| 久久欧美一区二区三区性牲奴| 中文字幕精品无码一区二区 | 奇米在线7777在线精品| 久久精品国产精油按摩| 国产女人好紧好爽| 国精产品一区一区三区| 八区精品色欲人妻综合网| 久久久久九九精品影院| 极品尤物一区二区三区|